I have Never seen the silvery coating in any 128,512, Ke, or Plus...
Neither have I. My eyes have only see the matte gray coating that feels slightly rough to the touch.

So was the coating on the inside of the case really that slick and shiny BEFORE you dipped it? Or was it originally the matte gray stuff but went shiny when you gave it the H202 bath?