I've had mixed experiences with retr0bright, I urge caution. It does what is advertised, but my problems have largely revolved around inconsistent de-yellowing resulting in blotchiness or streaking.
The typical recipes generate a sort of gel material, which if not mixed uniformly will not produce uniform results. Same problem with both uniform application and uniform exposure to UV/sunlight. In the future, I plan to try leaving out the gelling agents and mixing up enough to completely submerge the target plastic.
YMMV of course, just my suggestions from the couple batches I've made.
The typical recipes generate a sort of gel material, which if not mixed uniformly will not produce uniform results. Same problem with both uniform application and uniform exposure to UV/sunlight. In the future, I plan to try leaving out the gelling agents and mixing up enough to completely submerge the target plastic.
YMMV of course, just my suggestions from the couple batches I've made.