Post
The inside is gray, but it also has an oily/metallic look to it. Some of it is scraped away (from people opening/closing the case over the years) and it looks somewhat metallic. I don't want to destroy the inside. I'll post a picture... it's definitely pretty smooth, not 'rough' per se.
This is the kind of inside coating you want to avoid exposing to the H2O2 solution. It's smooth and shiny, and does not add to the thickness of the plastic.

macsig_inside_large.jpg.749de5eb12764e09b38300ebf414ece5.jpg


The "safe" kind is a matte finish, slightly rough to the touch, and tends to appear thicker than the casing.

20070312-signatures.jpg.0397c16867f9eb0d5821737b8507000d.jpg