True, and I don't always know what kind of metals I am dealing with, so my rule is to avoid metallic parts where possible when deyellowing. I don't remember exactly all the things I tested with RetroBright before I did my SE/30, but I noticed some RetroBright reaction on the metal parts affixed to the INSIDE of my HD20SC when I deyellowed it, but that was minor because it was only a few millimeters where the gel I used sploshed on some of the metal INSIDE the case (I wasn't trying to deyellow the inside). I also did not directly expose that "metal-parts" side of the HD20SC case to UV light either.